I applied Alumetron to my pontoon 4 years ago. Looks great, except for a few scuffs. I want to clean up the scuffs and reapply Alumetron again. what Is The process?

Can I use the boat wash and reapply? Should I scuff it with a scotch bright? How can I remove the abrasions before recoating? Will a topcoat over the previous coat stick well or peel off? Thank You for your help in advance.

PS Your product works great!

Answer:
For your convenience, I’ve highlighted the hyperlinks in case you want more information about the products.

Hi Joe,

I’m glad that you like our Alumetron®. after you repair the scuffs, you should get another 4 to 6 years of protection before you have to strip the Alumetron® and recoat. I’m happy that you like our products. Thanks for the compliment. We never get tired of hearing from our happy customers.

Scuffs are easy to repair in the Alumetron® coating. Abrasions in the aluminum can be a bit more tricky. 

DO NOT USE SCOTCH BRITE SCUFFING PADS. Your aluminum pontoons have a mill finish, which means that it has a fine grain that runs horizontally. If you scuff or scratch against the grain you will see scratch marks, swirls or additional scuff marks. Whenever cleaning, repairing, or coating, always work with the grain, never against it.

Use Alumabuff® and a Marine Power Mitt® to clean the scuffed area and remove any VS721® on the surface. Clean the area about 10 to 12 inches beyond the damaged area. If the scuffs are all the way through the Alumetron®, clean the aluminum until all the stains are removed and it’s restored. Remember; clean using horizontal, back and forth, motion so that you don’t create additional scuff marks or swirls. The Alumabuff® will remove VS721® and clean the exposed aluminum but will not remove the Alumetron®. 

If you have scratch marks, you can wet sand those out, if they’re not too deep, with 600 or 800 grit wet sandpaper on a longboard, or attached to a block of wood. Check a test spot on the inside of the pontoon to determine the right grit size to best match the original grain. Clean the area first as above.

If the scratches or dents are too deep, you’ll have to live with those. Sanding too deep will thin out the aluminum too much and pushing out dents is complicated and best left to an experienced professional. It entails drilling holes in the pontoon opposite the dent and banging them out, and then welding the holes shut or welding plates over the dents and then grinding the welds flush and refinishing the area. But, you’ll still see the repair.

After You’ve cleaned (and sanded if necessary) the damaged area, you can apply 4 coats of Alumetron® and after that’s cured, reapply the VS721®. The coating will blend in and will be invisible. When applying the Alumetron®, apply the 1st coat about 1″ to 2″ beyond the damaged area. Apply the 2nd coat about 1″ to 2″ beyond that. The 3rd coat another 1″ to 2″  and the final coat still another 1″ to 2″ beyond the last. In other words, feather it out so that it gets thinner as it overcoats the existing Alumetron®. 

Except for deep scratches or dents, the repair should be near invisible.